Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 945 MPa @Strain 0.200 % |
137000 psi @Strain 0.200 % |
Longitudinal, typical |
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Beta Forged Low Cost, Multipurpose Alloy. Tensile/toughness property data below for Beta Forged, RA material.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, but wi.. |
|||
Tensile Strength, Yield | 945 MPa @Temperature 25.0 °C |
137000 psi @Temperature 77.0 °F |
90°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, SGP196-PW Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 945 MPa @Strain 0.200 % |
137000 psi @Strain 0.200 % |
Longitudinal, typical |
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Alpha-Beta Forged, RA Low Cost, Multipurpose Alloy. Tensile/toughness property data below for Alpha-Beta Forged, RA material.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, .. |