Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 8.30 MPa @Strain 50.0 % |
1200 psi @Strain 50.0 % |
ASTM D412 |
GRECO ISOTHANE 1095AE Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are Poly(adipate)ester based thermoplastic polyurethanes with good balanced qualities. They exhibit good toughness, abrasive resistance, solvent resistance, and transp.. |
|||
Tensile Strength, Yield | 8.30 MPa @Strain 100 % |
1200 psi @Strain 100 % |
ASTM D412 |
GRECO ISOTHANE 3090AF Polyether TPU Resin ISOTHANE 3000F Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These pro.. |
|||
Tensile Strength, Yield | 8.30 MPa @Strain 100 % |
1200 psi @Strain 100 % |
ASTM D412 |
GRECO ISOTHANE 5090A Polyether TPU Resin ISOTHANE 5000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent bio-compatibility, hydrolytic resistance, fungus resistance, and low temperature performance pro.. |
|||
Tensile Strength, Yield | 8.30 MPa @Strain 300 % |
1200 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 2075A Poly(caprolactone)ester TPUÂ Resin ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi.. |
|||
Tensile Strength, Yield | 8.27 MPa @Strain 300 % |
1200 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Laripur® LPR 7560EG Thermoplastic Polyurethane Features: - Excellent performance under extreme and aggressive environments
- Superior abrasion and cut resistance
- Resistance to chemical, microbial attack and hydrolysis
- Excellent flexibility a.. |
|||
Tensile Strength, Yield | 8.27 MPa @Temperature 21.1 °C |
1200 psi @Temperature 70.0 °F |
Flatwise Tensile, Cured at 250°C for 60 min at 30 psi MMM-A-132 and MIL-A-25463. |
Hexcel® Redux® 382H (0.06 psf) Film Adhesive Redux 382H is a 250°F curing modified epoxy film adhesive available in both supported and unsupported versions. Redux 382H is a versatile adhesive system suitable for bonding a wide variety of subs.. |
|||
Tensile Strength, Yield | 8.30 MPa @Strain 300 % |
1200 psi @Strain 300 % |
ASTM D-412 |
BASF Elastollan® 1175AW Polyether Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes... |
|||
Tensile Strength, Yield | 8.30 MPa @Strain 300 % |
1200 psi @Strain 300 % |
ASTM D-412 |
BASF Elastollan® S80A Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fue.. |