Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 765 MPa @Temperature -55.0 °C |
111000 psi @Temperature -67.0 °F |
0°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 765 MPa @Temperature 93.3 °C |
111000 psi @Temperature 200 °F |
90°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 768 MPa @Strain 0.200 % |
111000 psi @Strain 0.200 % |
Typical for Plate, 1/4-Hard, Transverse, 0.1875" |
AK Steel NITRONIC® 30 Austenitic Stainless Steel AK Steel NITRONIC 30 Stainless Steel offers significantly higher strength than Type 304 and potential for applications requiring good resistance to aqueous and atmospheric corrosion resistance combi.. |
|||
Tensile Strength, Yield | 765 MPa @Strain 0.200 % |
111000 psi @Strain 0.200 % |
Longitudinal |
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition H 1150-M AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, .. |
|||
Tensile Strength, Yield | 765 MPa @Strain 0.200 % |
111000 psi @Strain 0.200 % |
Transverse |
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition H 1150-M AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, .. |
|||
Tensile Strength, Yield | 763 MPa @Strain 0.200 %, Thickness 25.4 mm |
111000 psi @Strain 0.200 %, Thickness 1.00 in |
Welded then age-hardened |
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |