Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 758 MPa @Strain 0.100 % |
110000 psi @Strain 0.100 % |
ASTM E345-93, Type A Specimen |
NiCoForm NiColoy® E Electroformed Nickel-Cobalt NiColoy® is a proprietary electrodeposited Nickel-Cobalt alloy distinguished by the following combination of features:Leveled, smooth matte to semi bright deposit with low internal stressHigh tensi.. |
|||
Tensile Strength, Yield | 759 MPa @Strain 0.200 %, Thickness 12.7 mm |
110000 psi @Strain 0.200 %, Thickness 0.500 in |
Welded then age-hardened |
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Tensile Strength, Yield | 759 MPa @Strain 0.200 %, Temperature 25.0 °C |
110000 psi @Strain 0.200 %, Temperature 77.0 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Tensile Strength, Yield | 758 - 889 MPa @Strain 0.200 %, Thickness >=25.4 mm |
110000 - 129000 psi @Strain 0.200 %, Thickness >=1.00 in |
Cold Drawn Bars |
Schmolz + Bickenbach 416RS Stainless Steel Bar Description: Ugitech’s 416RS is a low sulfur pre-hardened chrome bearing martensitic stainless steel specifically designed for the precision rifle barrel industry. The 416RS chemistry is balanc.. |
|||
Tensile Strength, Yield | 758 MPa @Strain 0.200 % |
110000 psi @Strain 0.200 % |
Cold-Worked 1/2 hard |
AK Steel 201 Austenitic Stainless steel AK Steel 210 was developed originally to conserve nickel. It provides properties similar to Type 301 and can be used in most applications for Type 301. This alloy is non-magnetic in the annealed c.. |
|||
Tensile Strength, Yield | 758 MPa @Strain 0.200 % |
110000 psi @Strain 0.200 % |
Cold-Worked 1/2 hard |
AK Steel 201LN Austenitic Stainless steel AK Steel 210 was developed originally to conserve nickel. It provides properties similar to Type 301 and can be used in most applications for Type 301. This alloy is non-magnetic in the annealed c.. |
|||
Tensile Strength, Yield | 758 MPa @Strain 0.200 % |
110000 psi @Strain 0.200 % |
Cold-Worked 1/2 hard |
AK Steel 301 Austenitic Stainless steel AK Steel 301 provides high strength and good ductility when cold worked. It is a modification of AK Steel 302 to increase the cold work-hardening range, to permit higher tensile strengths to be ach.. |
|||
Tensile Strength, Yield | 759 MPa @Strain 0.200 % |
110000 psi @Strain 0.200 % |
Typical for Plate, 1/4-Hard, Transverse, 0.25" |
AK Steel NITRONIC® 30 Austenitic Stainless Steel AK Steel NITRONIC 30 Stainless Steel offers significantly higher strength than Type 304 and potential for applications requiring good resistance to aqueous and atmospheric corrosion resistance combi.. |
|||
Tensile Strength, Yield | 758 MPa @Strain 0.200 %, Thickness 12.7 mm |
110000 psi @Strain 0.200 %, Thickness 0.500 in |
Welded then age-hardened |
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |
|||
Tensile Strength, Yield | 758 MPa @Temperature 23.0 °C |
110000 psi @Temperature 73.4 °F |
|
ATI Wah Chang TI-3Al-2.5V Ti-3Al-2.5V has proved to be a sufficiently malleable material for tube manufacture. It can be cold worked by standard tube making processes, is weldable and can be strength-ended by cold working an.. |