Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 7.60 MPa @Strain 100 % |
1100 psi @Strain 100 % |
ASTM D412 |
GRECO ISOTHANE 1190A Poly(adipate)ester TPUÂ Resin ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp.. |
|||
Tensile Strength, Yield | 7.60 MPa @Strain 50.0 % |
1100 psi @Strain 50.0 % |
ASTM D412 |
GRECO ISOTHANE 1195A Poly(adipate)ester TPUÂ Resin ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp.. |
|||
Tensile Strength, Yield | 7.60 MPa @Strain 50.0 % |
1100 psi @Strain 50.0 % |
ASTM D412 |
GRECO ISOTHANE 1090A Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tensile Strength, Yield | 7.58 MPa @Temperature -55.0 °C |
1100 psi @Temperature -67.0 °F |
Flatwise Tensile, Cured at 250°C for 60 min at 30 psi MMM-A-132 and MIL-A-25463. |
Hexcel® Redux® 382H (0.06 psf) Film Adhesive Redux 382H is a 250°F curing modified epoxy film adhesive available in both supported and unsupported versions. Redux 382H is a versatile adhesive system suitable for bonding a wide variety of subs.. |
|||
Tensile Strength, Yield | 7.60 MPa @Strain 100 % |
1100 psi @Strain 100 % |
ASTM D-412 |
BASF Elastollan® 1185A10X Wire & Cable Grade Polyurethane Elastomer Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Tensile Strength, Yield | 7.60 MPa @Strain 100 % |
1100 psi @Strain 100 % |
ASTM D-412 |
BASF Elastollan® 1185A Polyether Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes... |
|||
Tensile Strength, Yield | 7.60 MPa @Strain 100 % |
1100 psi @Strain 100 % |
ASTM D-412 |
BASF Elastollan® 1185A10U Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Tensile Strength, Yield | 7.60 MPa @Strain 100 % |
1100 psi @Strain 100 % |
ASTM D-412 |
BASF Elastollan® 1185A10V Wire & Cable Grade Polyurethane Elastomer Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Tensile Strength, Yield | 7.55 MPa @Strain 300 % |
1100 psi @Strain 300 % |
ASTM D412 |
SK Chemicals SKYTHANE® 400 Hotmelt Grade UB Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |