Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 330 MPa @Strain 1.00 % |
47900 psi @Strain 1.00 % |
Outokumpu Typical,Cold Rolled Strip/Sheet; EN 10002-1 |
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Yield | 330 MPa @Strain 1.00 % |
47900 psi @Strain 1.00 % |
Outokumpu Typical,Cold Rolled Strip/Sheet; EN 10002-1 |
Outokumpu 4310 Cr-Ni Austenitic Stainless Steel Cold work hardening steel suitable for manufacture of springs operating in corrosive conditions.Available hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and ro.. |
|||
Tensile Strength, Yield | 330 MPa @Strain 0.200 %, Temperature 100 °C |
47900 psi @Strain 0.200 %, Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu SAF 2304® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Tensile Strength, Yield | >= 330 MPa @Strain 1.00 % |
>= 47900 psi @Strain 1.00 % |
|
Industeel URANUS® B25 6 Mo Cost Saving Super-Austenitic Stainless Steel with PREN = 42 Description: URANUS® B25 (UR B25) is a 18% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed to be cost effective. The 18% nickel and 0... |
|||
Tensile Strength, Yield | 330 MPa @Temperature 177 °C |
47900 psi @Temperature 351 °F |
|
Hexcel® F161 Epoxy Resin, 7781 Glass Fabric Hexcel designation: 7781-38"-F161; Fiber: 75-1/0Information provided by HexCel |
|||
Tensile Strength, Yield | 330 MPa @Temperature 93.0 °C |
47900 psi @Temperature 199 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, 220 Glass Fabric Information provided by HexCel |
|||
Tensile Strength, Yield | 330 MPa @Strain 0.200 %, Thickness 152.4 - 203.2 mm |
47900 psi @Strain 0.200 %, Thickness 6.000 - 8.000 in |
Typical Strength |
Constellium Alumold® 350 Aluminum Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti.. |
|||
Tensile Strength, Yield | >= 330 MPa @Strain 0.200 %, Thickness 203.2 - 254 mm |
>= 47900 psi @Strain 0.200 %, Thickness 8.000 - 10.0 in |
Tempers T651 / T652 |
Constellium Alumold® 400 Aluminum The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds.. |
|||
Tensile Strength, Yield | >= 330 MPa @Strain 0.200 %, Thickness 60.0 - 80.0 mm |
>= 47900 psi @Strain 0.200 %, Thickness 2.36 - 3.15 in |
Temper T651 |
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing .. |
|||
Tensile Strength, Yield | >= 330 MPa @Strain 0.200 %, Thickness 80.0 - 120 mm |
>= 47900 psi @Strain 0.200 %, Thickness 3.15 - 4.72 in |
Temper T651 |
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing .. |
|||
Tensile Strength, Yield | 330 MPa @Strain 1.00 % |
47900 psi @Strain 1.00 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 4948 High Temperature Austenitic Stainless Steel Creep-resistant variant of 1.4301, with a standardized minimum carbon content for service at temperatures of up to 800°C in dry air.Applications: Heat and creep resistance. For use over 550°C for.. |
|||
Tensile Strength, Yield | 330 MPa @Strain 0.200 %, Temperature 200 °C |
47900 psi @Strain 0.200 %, Temperature 392 °F |
EN min.; EN 10002-5 |
Outokumpu LDX 2101® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |