Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 268 MPa @Temperature 93.0 °C |
38800 psi @Temperature 199 °F |
|
ATI Wah Chang Zircadyne® Alloy Zr 702 Zircadyne 702 is commercially pure zirconium. Alloy exhibits good ductility even at cryogenic temperatures and good strength comparable with other common engineering alloys.Information provided by A.. |
|||
Tensile Strength, Yield | 268 MPa @Thickness 19.1 mm, Temperature 204 °C |
38900 psi @Thickness 0.752 in, Temperature 399 °F |
0.2% Offset |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Plate, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |