Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 140 MPa @Strain 0.200 %, Temperature 100 °C |
20300 psi @Strain 0.200 %, Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu 4845 High Temperature Austenitic Stainless Steel Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o.. |
|||
Tensile Strength, Yield | 140 MPa @Temperature -10.0 °C |
20300 psi @Temperature 14.0 °F |
ASTM D638 |
Gharda Chemicals G-PAEKâ„¢ 1200G Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in colorApplication Areas:.. |
|||
Tensile Strength, Yield | 140 MPa @Strain 0.200 %, Thickness 20.0 - 150 mm |
20300 psi @Strain 0.200 %, Thickness 0.787 - 5.91 in |
Typical Strength |
Constellium PLAN 5083 Aluminum Rolled Plate Rolled plates in 5083 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5083 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m.. |
|||
Tensile Strength, Yield | 140 MPa @Strain 0.200 %, Thickness 20.0 - 150 mm |
20300 psi @Strain 0.200 %, Thickness 0.787 - 5.91 in |
Typical Strength |
Constellium PLAN 5754 Aluminum Rolled Plate Rolled plates in 5754 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5754 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m.. |
|||
Tensile Strength, Yield | 140 MPa @Strain 0.200 %, Thickness 20.0 - 150 mm |
20300 psi @Strain 0.200 %, Thickness 0.787 - 5.91 in |
Typical Strength |
Constellium PLAN OX 5754 Aluminum Rolled Plate Rolled plates in 5754 PLAN OX are optimized for minimum residual stress, improved dimensional tolerances and for decorative* anodizing. 5754 PLAN OX is mainly used for low stressed, anodized compone.. |
|||
Tensile Strength, Yield | 140 MPa @Strain 0.200 %, Thickness 20.0 - 100 mm |
20300 psi @Strain 0.200 %, Thickness 0.787 - 3.94 in |
Typical Strength |
Constellium Planoxal® 50 Aluminum plate Planoxal®-50 plates differ from other standard EN-AW 5083 alloy products by their low level of residual stress. This specialty plate is also suitable for decorative anodizing. Planoxal®-50 is main.. |
|||
Tensile Strength, Yield | 140 MPa @Temperature 80.0 °C |
20300 psi @Temperature 176 °F |
|
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |