Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 11.0 MPa @Strain 300 % |
1600 psi @Strain 300 % |
DIN 53.504 |
Lubrizol Advanced Materials Pearlcoat® 125KW Thermoplastic Polyurethane Elastomer
(discontinued **) Pearlcoat® D125KW is a polyester-based aromatic TPU, supplied in form of white-colored pellets, combining hardness with excellent low-temperature flexibility.Applications: Pearlcoat® D125KW is us.. |
|||
Tensile Strength, Yield | 11.0 MPa @Strain 100 % |
1600 psi @Strain 100 % |
ASTM D412 |
GRECO ISOTHANE 1198A Poly(adipate)ester TPUÂ Resin ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp.. |
|||
Tensile Strength, Yield | 11.0 MPa @Strain 100 % |
1600 psi @Strain 100 % |
ASTM D412 |
GRECO ISOTHANE 2095A Poly(caprolactone)ester TPUÂ Resin ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi.. |
|||
Tensile Strength, Yield | 11.0 MPa @Strain 300 % |
1600 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 3080A Polyether TPU Resin ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod.. |
|||
Tensile Strength, Yield | 11.0 MPa @Strain 300 % |
1600 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 3080AF Polyether TPU Resin ISOTHANE 3000F Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These pro.. |
|||
Tensile Strength, Yield | 11.0 MPa @Strain 100 % |
1600 psi @Strain 100 % |
ASTM D412 |
GRECO ISOTHANE 3095A Polyether TPU Resin ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod.. |
|||
Tensile Strength, Yield | 11.0 MPa @Strain 300 % |
1600 psi @Strain 300 % |
ASTM D412 |
GRECO ISOTHANE 1080A Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tensile Strength, Yield | 11.0 MPa @Strain 100 % |
1600 psi @Strain 100 % |
ASTM D412 |
GRECO ISOTHANE 1095A Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tensile Strength, Yield | 11.0 MPa @Strain 300 % |
1600 psi @Strain 300 % |
0.76 mm (0.030 in) extruded sheet; ASTM D-412 |
BASF Elastollan® 1175A10W Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Tensile Strength, Yield | 11.0 MPa @Strain 100 % |
1600 psi @Strain 100 % |
ASTM D-412 |
BASF Elastollan® S90A Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fue.. |
|||
Tensile Strength, Yield | 11.0 MPa @Strain 300 % |
1600 psi @Strain 300 % |
ASTM D-412 |
BASF Elastollan® 685A10 Polyester Type Polyurethane Elastomer This grade contains a hydrolytic stabilizer. The Elastollan 600 Series of products listed are products that are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are .. |