Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : K (wear) Factor = 70.0 x 10-10 in³-min/ft-lb-hr Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 141 x 10-8 mm³/N-M
70.0 x 10-10 in³-min/ft-lb-hr
40psi, 50ft/min; tested in accordance with LNP WI-0687
LNP Stat-Kon® EC-1008 EM BK8-115 Polyetherimide, Carbon Fiber Reinforcement  (discontinued **)
Features: Electrically Conductive, Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; howev..
K (wear) Factor 141 x 10-8 mm³/N-M
70.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY RF203 PA 66 (Europe-Africa-Middle East)
LNP* LUBRILOY* RF203 is a compound based on PA 66 resin containing Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated.
K (wear) Factor 141 x 10-8 mm³/N-M
70.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY RF203H PA 66
LNP LUBRILOY* RF203H is a compound based on Nylon 66 resin containing 15% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare.
K (wear) Factor 141 x 10-8 mm³/N-M
70.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY RF203XXH PA 66
LNP* LUBRILOY* RF203XXH is a compound based on Nylon 66 resin containing 15% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare.
K (wear) Factor 141 x 10-8 mm³/N-M
70.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D 3702 Modified
SABIC Innovative Plastics LNP Stat-kon EE008E PEI (Asia Pacific)
LNP STAT-KON* EE008E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pacif..
K (wear) Factor 141 x 10-8 mm³/N-M
70.0 x 10-10 in³-min/ft-lb-hr
Techmer ES Luriblend® PPS/F GF30 TL15 BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionAppearance: BlackIn..
K (wear) Factor 141 x 10-8 mm³/N-M
70.0 x 10-10 in³-min/ft-lb-hr
Thrust washer at 2000 PV
Techmer ES Plaslube® J-4/30/TF/15 Nylon 612, 30% GFR, 15% PTFE
Plaslube glass fiber reinforced polytetrafluoroethylene (PTFE) lubricated nylon 612 grades offer a unique balance of excellent wear and friction performance with good dimensional stability and mecha..