Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | >= 2010 x 10-8 mm³/N-M | >= 1000 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Quadrant PPSU LSG PPSU, Extruded, Unfilled, Polyphenylsulfone (ASTM Product Data Sheet) |
|||
K (wear) Factor | >= 2010 x 10-8 mm³/N-M | >= 1000 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Semitron® CMP XL20 (ASTM Product Data Sheet) |
|||
K (wear) Factor | 2010 x 10-8 mm³/N-M | 1000 x 10-10 in³-min/ft-lb-hr | PV=2000 psi-fpm vs Self; SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC LNP* Stat-kon* Lexan_LC1500N compound is a 15% carbon fiber, 6% PTFE reinforced polycarbonate. |
|||
K (wear) Factor | 2010 x 10-8 mm³/N-M | 1000 x 10-10 in³-min/ft-lb-hr | PV=2000 psi-fpm vs Self; SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC (Europe-Africa-Middle East) LNP* Stat-kon* Lexan_LCF1506 is a 15% carbon fiber, 6% PTFE reinforced polycarbonate. |
|||
K (wear) Factor | 2010 x 10-8 mm³/N-M | 1000 x 10-10 in³-min/ft-lb-hr | PV=2000 psi-fpm vs Self; SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC (Asia Pacific) 15% carbon fiber, 6% PTFE reinforced polycarbonate. |