Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 181 x 10-8 mm³/N-M | 90.0 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Nylatron® GS Nylon, Extruded MoS2 Filled Type 66 (ASTM Product Data Sheet) |
|||
K (wear) Factor | 181 x 10-8 mm³/N-M | 90.0 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Nylatron® GSM Nylon, Cast MoS2 Filled Type 6 (ASTM Product Data Sheet) |
|||
K (wear) Factor | 181 x 10-8 mm³/N-M | 90.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DBL349E PC (Asia Pacific) LNP* Lubricomp* DBL349E is a compound based on Polycarbonate resin containing Glass Bead, PTFE, Flame Retardant. Added features of this material include:LNP* Lubricomp* DBL349E is a compound based .. |
|||
K (wear) Factor | 181 x 10-8 mm³/N-M | 90.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DBL349E PC LNP* Lubricomp* DBL349E is a compound based on Polycarbonate resin containing 20% Glass Bead, 15% PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retard.. |