Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 111 x 10-8 mm³/N-M | 55.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP DL0029E PC LNP LUBRICOMP* DL0029E is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Internally Lubricated, Flame Retardant. |
|||
K (wear) Factor | 111 x 10-8 mm³/N-M | 55.0 x 10-10 in³-min/ft-lb-hr | 40psi, 50ft/min; tested in accordance with LNP WI-0687 |
LNP Thermocomp® LC-1006 Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
K (wear) Factor | 111 x 10-8 mm³/N-M | 55.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP THERMOCOMP LC006 PEEK LNP THERMOCOMP* LC006 is a compound based on Polyetheretherketone resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
K (wear) Factor | 111 x 10-8 mm³/N-M | 55.0 x 10-10 in³-min/ft-lb-hr | ASTM D3702 |
Ensinger Delrin® 150 Homopolymer Acetal (POM) Ensinger's Delrin® 150 stock shapes are a homopolymer acetal manufactured using DuPont Delrin 150 Resin. It is a crystalline plastic which offers an excellent balance of properties to bridge the g.. |