Polymer Property : Flexural Modulus, 1% Secant = 190000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1310 MPa
190000 psi
0.05 in/min; ASTM D790A
ExxonMobil AP03B Polypropylene Impact Copolymer
Product Description: A high crystallinity, medium impact copolymer resin with high melt flow rate and excellent processing attributes. It is designed for injection molded large appliance applicatio..
Flexural Modulus, 1% Secant 1310 MPa
190000 psi
ASTM D790B
ExxonMobil HDPE HD 6704.18 High Density Polyethylene Copolymer Resin
Product Description: HD 6704 is a narrow molecular weight hexane copolymer designed for outstanding balance of ESCR, Toughness and Stiffness properties. This resin is ideally suited for heavy-duty a..
Flexural Modulus, 1% Secant 1310 MPa
190000 psi
ASTM D790B
ExxonMobil HDPE HD 6706.17 High Density Polyethylene Copolymer Resin
Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su..
Flexural Modulus, 1% Secant 1310 MPa
190000 psi
ASTM D790B
ExxonMobil HDPE HD 6706.62 High Density Polyethylene Copolymer Resin
Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su..
Flexural Modulus, 1% Secant 1310 MPa
190000 psi
ASTM D790A
Dow 5D98 Polypropylene Homopolymer Resin
OverviewConsistent processabilityGood optical propertiesHigh strength propertiesComplies with: U.S. FDA 21 CFR 177.1520 (c)1.1a, Europe EU-Directive 2002/72/ECDOW 5D98 Polypropylene Resin is intende..
Flexural Modulus, 1% Secant 1310 MPa
190000 psi
ASTM D790
ExxonMobil HD 6704.18 Injection Molding Resin
Product Description: HD 6704 is a narrow molecular weight hexane copolymer designed for outstanding balance of ESCR, Toughness and Stiffness properties. This resin is ideally suited for heavy-duty a..
Flexural Modulus, 1% Secant 1310 MPa
190000 psi
ASTM D790
ExxonMobil HD 6706.17 Injection Molding Resin
Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su..
Flexural Modulus, 1% Secant 1310 MPa
190000 psi
ASTM D790
ExxonMobil HD 6706.62 Injection Molding Resin
Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su..