Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1310 MPa | 190000 psi | 0.05 in/min; ASTM D790A |
ExxonMobil AP03B Polypropylene Impact Copolymer Product Description: A high crystallinity, medium impact copolymer resin with high melt flow rate and excellent processing attributes. It is designed for injection molded large appliance applicatio.. |
|||
Flexural Modulus, 1% Secant | 1310 MPa | 190000 psi | ASTM D790B |
ExxonMobil HDPE HD 6704.18 High Density Polyethylene Copolymer Resin Product Description: HD 6704 is a narrow molecular weight hexane copolymer designed for outstanding balance of ESCR, Toughness and Stiffness properties. This resin is ideally suited for heavy-duty a.. |
|||
Flexural Modulus, 1% Secant | 1310 MPa | 190000 psi | ASTM D790B |
ExxonMobil HDPE HD 6706.17 High Density Polyethylene Copolymer Resin Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su.. |
|||
Flexural Modulus, 1% Secant | 1310 MPa | 190000 psi | ASTM D790B |
ExxonMobil HDPE HD 6706.62 High Density Polyethylene Copolymer Resin Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su.. |
|||
Flexural Modulus, 1% Secant | 1310 MPa | 190000 psi | ASTM D790A |
Dow 5D98 Polypropylene Homopolymer Resin OverviewConsistent processabilityGood optical propertiesHigh strength propertiesComplies with: U.S. FDA 21 CFR 177.1520 (c)1.1a, Europe EU-Directive 2002/72/ECDOW 5D98 Polypropylene Resin is intende.. |
|||
Flexural Modulus, 1% Secant | 1310 MPa | 190000 psi | ASTM D790 |
ExxonMobil HD 6704.18 Injection Molding Resin Product Description: HD 6704 is a narrow molecular weight hexane copolymer designed for outstanding balance of ESCR, Toughness and Stiffness properties. This resin is ideally suited for heavy-duty a.. |
|||
Flexural Modulus, 1% Secant | 1310 MPa | 190000 psi | ASTM D790 |
ExxonMobil HD 6706.17 Injection Molding Resin Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su.. |
|||
Flexural Modulus, 1% Secant | 1310 MPa | 190000 psi | ASTM D790 |
ExxonMobil HD 6706.62 Injection Molding Resin Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su.. |