Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 27.0 MPa @Temperature 145 °C, Time 2990 sec |
3920 psi @Temperature 293 °F, Time 0.830 hour |
cured; ASTM D412 |
LG Chemical NBR 6230 High Acrylonitrile Polymer Description: NBR 6230 is a copolymer of butadiene and acrylonitrile manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 6230 is a non staining, low mooney, and m.. |
|||
Tensile Strength at Break | 27.0 MPa @Temperature 150 °C |
3920 psi @Temperature 302 °F |
|
LATI Latiblend 6252 H2 G/30 PA6/PP Homopolymer Blend based on Polyamide 6 (PA6) / Polypropylene homopolymer (PPh). Heat stabilized. Glass fibers. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |