Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 240 MPa @Temperature 23.0 °C |
34800 psi @Temperature 73.4 °F |
ISO 527 |
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac.. |
|||
Tensile Strength at Break | 240 MPa @Temperature 23.0 °C |
34800 psi @Temperature 73.4 °F |
|
LATI Larpeek 10 K/30 PEEK, 30% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Strength at Break | 240 MPa @Temperature 90.0 °C |
34800 psi @Temperature 194 °F |
|
LATI Larpeek 10 K/40 PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Tensile Strength at Break | 240 MPa @Temperature 60.0 °C |
34800 psi @Temperature 140 °F |
|
LATI Laramid G/60 PPA, 60% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Tensile Strength at Break | 240 MPa @Temperature 23.0 °C |
34800 psi @Temperature 73.4 °F |
|
LATI Latigloss 57 G/50 F2 PPA, 50% Glass Fiber Reinforced Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact application. Availability: .. |
|||
Tensile Strength at Break | 240 MPa @Temperature 982 °C |
34800 psi @Temperature 1800 °F |
Plate; Longitudinal |
Special Metals INCONEL® alloy MA758 Ni-Cr Superalloy INCONEL® alloy MA 758 is an oxide-dispersion-strengthened (ODS) nickel-chromium superalloy, made by mechanical alloying. It is a development of the well-established aerospace superalloy, INCONEL.. |
|||
Tensile Strength at Break | 240 MPa @Temperature 23.0 °C |
34800 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |