Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS (Europe-Africa-Middle East) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Eur.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 104 PC (Europe-Africa-Middle East) LEXAN 104 is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatibility informati.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 244R PC (Europe-Africa-Middle East) LEXAN 244R resin grade is a medium viscosity multi purpose product with improved flame resistance and release properties. It is also US FDA food contact compliant available in limited colorsThis dat.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 945ASR PC Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® AD4820 PC LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin.This data was supplied by SABIC-IP for the America.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD103 PC (Asia Pacific) FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the .. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD103 PC (Europe-Africa-Middle East) FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the .. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD104R PC (Europe-Africa-Middle East) FXD104R is a Light Diffusion effect, which is part of the VisualFX family. Color Package may affect properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD141 PC (Europe-Africa-Middle East) LEXAN FXD141 is a transparent/translucent medium viscosity grade for light diffusion effects. The color package may affect performance.This data was supplied by SABIC-IP for the Europe-Africa-Middl.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD951A PC Visual effetcs diffusion, flame retardant PC with low/medium flow good for extrusion/injection molding applications. Ideal for light management platforms that require hiding power and transmission.T.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD9945A PC UV stabilzed Visualfx FR PC with non-brominated and non-chlorinated flame retardant systems. It is available Only in white diffused effect(WH8B111X) meeting UL-94 V0 at 2mm for thin wall application.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXE101 PC (Europe-Africa-Middle East) Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). For thicker sections without sinks.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® GLX143 PC (Europe-Africa-Middle East) Lexan* GLX resin is a medium viscosity grade which is an excellent candidate for applications with high optical quality requirements, such as automotive glazing applications. Available in transparen.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPM1914 PC Copolymer (Europe-Africa-Middle East) High flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). E.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® OQ2220 PC Ophthalmic/safety lens market. OQ2xxx series in all transparent tints. Dedicated equipment, stringent production control conditions.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® SLX2531T PC Copolymer (Europe-Africa-Middle East) Transparent weatherable PC copolymer for blowmolding/extrusion.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
DuPont Performance Polymers Crastin® ST830FRUV NC010 PBT
(Unverified Data**) Crastin® ST830FRUV NC010 is an unreinforced, Super Tough, flame retardant polybutylene terephthalate resin for injection molding. It contains a UV light stabilizer and is recognized as UL94V-0 at 0.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXRL0662 PC Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXD144R PC (Europe-Africa-Middle East) LEXAN FXD144R is a transparent/translucent medium viscosity grade for light diffusion effects. FDA compliant. Internal mold release. The color package may affect performance.This data was supplie.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
Mitsubishi Xantar® MX 1021 FD MX 1021 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics PC0700 PC (Europe-Africa-Middle East) PC0700 resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics PC0800 PC PC0800 resin is a low flow (MFR = 8 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics PC1000R PC PC1000R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplie.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics PC1003R PC PC1003R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was .. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics PC1800R PC (Asia Pacific) PC1800R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecotek® PC30 NL RX PC, unfilled, improved flow & low temperature impact, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXE144H PC (Europe-Africa-Middle East) FXE144H is a Lexan PC Translucent Grade in our VisualFX Portfolio. It is part of Energy family, which includes Illuminate, Glass, and Flame effects. Grade was developed to meet the Aesthetic Differe.. |
|||
Izod Impact, Notched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
ISO 180/4A |
Mitsubishi Xantar® C CM 506 Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |