Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 48.0 kJ/m² @Temperature 23.0 °C |
22.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1484T PC Copolymer Lexan* EXL1484T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in c.. |
|||
Izod Impact, Notched (ISO) | 48.0 kJ/m² @Temperature 23.0 °C |
22.8 ft-lb/in² @Temperature 73.4 °F |
12.7-mm x 3.2-mm, 0.25-mm notch; ASTM-D256 |
Ineos ABS Lustran® Guardian™ 682 ABS, Injection Molding Grade Lustran® ABS 682 is a high performance, HCFC-141b resistant grade of ABS for injection molded refrigerator and freezer components. |
|||
Izod Impact, Notched (ISO) | 48.0 kJ/m² @Temperature 23.0 °C |
22.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
LyondellBasell Hifaxâ„¢ CB251 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB251 medium melt flow, 1,200 MPa flexural modulus, low CLTE, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of impact resis.. |
|||
Izod Impact, Notched (ISO) | 48.0 kJ/m² @Temperature 23.0 °C |
22.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
LyondellBasell Hifaxâ„¢ HSBMG265 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ HSBMG265 medium high melt flow, 1,400 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent combination of rigidity, .. |
|||
Izod Impact, Notched (ISO) | 48.0 kJ/m² @Temperature 23.0 °C |
22.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180-A |
Covestro Bayblend® M850 XF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Eas.. |
|||
Izod Impact, Notched (ISO) | 48.0 kJ/m² @Temperature 23.0 °C |
22.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180-A |
Covestro Bayblend® T65 HI PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Improve low temperature .. |
|||
Izod Impact, Notched (ISO) | 48.0 kJ/m² @Temperature 23.0 °C |
22.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180-A |
Covestro Bayblend® W85 HI PC ASA Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Imp.. |
|||
Izod Impact, Notched (ISO) | 48.0 kJ/m² @Temperature 23.0 °C |
22.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Dow T702-12N Polypropylene Impact Copolymer Resin Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011. |