Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched (ISO) = 60.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-..
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer (Asia Pacific)
Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h..
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h..
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL6414 PC (Europe-Africa-Middle East)
PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® FXE174R PC (Europe-Africa-Middle East)
LEXAN FXE174R is a high flow visualFx Energy grade, suitable for steam sterilization and compliant with medical and food contact regulations. This material is especially developed for applications t..
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer
Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac..
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer (Asia Pacific)
Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac..
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HPS2S PC
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza..
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Europe-Africa-Middle East)
Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o..
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® LSHF PC
Clear PolyCarbonate, High Flow, UV Stabilization, Heat StabilizationThis data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® ML6413 PC (Europe-Africa-Middle East)
Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope..
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer (Asia Pacific)
Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi..
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi..
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer
Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h..
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer (Europe-Africa-Middle East)
Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac..
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature -20.0 °C
28.6 ft-lb/in²

@Temperature -4.00 °F
ISO 180/4A
DSM Stapron® E EM 605 Polycarbonate/PET Blend (European Grade)  (discontinued **)
Information provided by DSM.
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature -20.0 °C
28.6 ft-lb/in²

@Temperature -4.00 °F
ISO 180/4A
Mitsubishi Xantar® C CM 506 U Polycarbonate/ABS Blend
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature -20.0 °C
28.6 ft-lb/in²

@Temperature -4.00 °F
ISO 180/4A
Mitsubishi Xantar® MX 1020 Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature -20.0 °C
28.6 ft-lb/in²

@Temperature -4.00 °F
ISO 180/4A
Mitsubishi Xantar® MX 1021 FD MX 1021 Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature -20.0 °C
28.6 ft-lb/in²

@Temperature -4.00 °F
ISO 180/4A
Mitsubishi Xantar® MX 1021 FD Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1eA
Solvay TECHNYL® A 246M PA66, DRY
Description: Unreinforced and modified polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHN..
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 180-A
Covestro Makroblend® UT5207 PC/PBT Blend
Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• Impact modified•..
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature -20.0 °C
28.6 ft-lb/in²

@Temperature -4.00 °F
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® FN718 BK230A Nylon 66  (Unverified Data**)
Zytel® FN718 BK230A is a flexible, plasticizer free modified black polyamide 66 resin having good heat aging and chemical resistance.Information provided by DuPont Performance Polymers
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 180-A
Covestro Makroblend® UT5205 PC/PBT Blend
Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• Impact modified•..
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Eurotec® Tecolen® CP30 NL XC30 PPCP, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec®
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Eurotec® Tecotek® BC40 UF45 NL CE PC/ABS, unfilled, heat & UV stabilized, natural, easy flow grade
Information provided by Eurotec®
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ASTM D256
BASF Ultramid® 8202 L Intermediate PA6 (Dry)
Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai..
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature -20.0 °C
28.6 ft-lb/in²

@Temperature -4.00 °F
ISO 180/4A
Mitsubishi Xantar® C CE 407 Polycarbonate/ABS Blend
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher..
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature -20.0 °C
28.6 ft-lb/in²

@Temperature -4.00 °F
ISO 180/4A
Mitsubishi Xantar® C CM 506 Polycarbonate/ABS Blend
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher..
Izod Impact, Notched (ISO) 60.0 kJ/m²

@Temperature 23.0 °C
28.6 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Polyram RamSter PF801 PBT, High Impact Modified
High impact modified PBT for injection molding applications.Information provided by Polyram.
Copyright © lookpolymers.com All Rights Reserved