Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 26.0 kJ/m² @Temperature 0.000 °C |
12.4 ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Geloy XTPMFR15 ASA+PC (Europe-Africa-Middle East) Geloy XTPMFR15 is a chlorine and bromine free flame retardant ASA/PC blend with improved impact performance/ductility and an UL94 rating of V0 at 1.5mm. This grade has a f1 rating according UL746C.T.. |
|||
Izod Impact, Notched (ISO) | 26.0 kJ/m² @Temperature -10.0 °C |
12.4 ft-lb/in² @Temperature 14.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Geloy XTPM307 ASA+PC (Europe-Africa-Middle East) XTPM307 is a high heat resistant PC/ASA with improved processing stability over HRA150. Typical values measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Izod Impact, Notched (ISO) | 26.0 kJ/m² @Temperature -10.0 °C |
12.4 ft-lb/in² @Temperature 14.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Geloy XTPM309E ASA+PC (Europe-Africa-Middle East) XTPM309E is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour stab.. |
|||
Izod Impact, Notched (ISO) | 26.0 kJ/m² @Temperature 23.0 °C |
12.4 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
LyondellBasell Hifaxâ„¢ CB247G Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB247G high melt flow, 1,700 MPa flexural modulus, UV-stabilized, weatherable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of propert.. |
|||
Izod Impact, Notched (ISO) | 26.0 kJ/m² @Temperature 23.0 °C |
12.4 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Styron MAGNUMâ„¢ 1250 BG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Impact, High Heat, Blow Molding ABSInformation provided by Styron |
|||
Izod Impact, Notched (ISO) | 26.0 kJ/m² @Temperature -40.0 °C |
12.4 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® XD549S PBT+PC (Europe-Africa-Middle East) Xenoy XD549S is an automotive grade, designed for thin wall (2.5 mm.) direct gated exterior parts. The material has an excellent flow. Xenoy XD549S can be painted with primerless solvent or waterbas.. |
|||
Izod Impact, Notched (ISO) | 26.0 kJ/m² @Temperature 23.0 °C |
12.4 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Verton NV0081EV_GY7E149 PC+ABS Preliminary data for 40% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 26.0 kJ/m² @Temperature 23.0 °C |
12.4 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**) Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide.. |