Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 1.00 kJ/m² @Temperature 23.0 °C |
0.476 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® INP564 ABS SABIC INP564 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Izod Impact, Notched (ISO) | 1.00 kJ/m² @Temperature 23.0 °C |
0.476 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® INP576 ABS Can be used as compounding additives for polymer blends. Medium molecular weight SAN. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for direc.. |
|||
Izod Impact, Notched (ISO) | 1.00 kJ/m² @Temperature -30.0 °C |
0.476 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® INP576 ABS Can be used as compounding additives for polymer blends. Medium molecular weight SAN. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for direc.. |
|||
Izod Impact, Notched (ISO) | 1.00 kJ/m² @Temperature 23.0 °C |
0.476 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® INP581 ABS High flow, low molecular weight SAN.
Can be used as compounding additives for polymer blends.
Can be blended with high rubber graft modifier resins to produce customized ABS properties.
Suitable for.. |
|||
Izod Impact, Notched (ISO) | 1.00 kJ/m² @Temperature -30.0 °C |
0.476 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® INP581 ABS High flow, low molecular weight SAN.
Can be used as compounding additives for polymer blends.
Can be blended with high rubber graft modifier resins to produce customized ABS properties.
Suitable for.. |
|||
Izod Impact, Notched (ISO) | 1.00 kJ/m² @Temperature -30.0 °C |
0.476 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® INP630 ABS INP630 is a specialty polymer that increases the service temperature of products. Can be used with a impact modifier to provide impact strength as well as high heat resistance.
Provides excellent hi.. |
|||
Izod Impact, Notched (ISO) | 1.00 kJ/m² @Temperature -30.0 °C |
0.476 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl PKN4766 PPE+HIPS (Europe-Africa-Middle East) NORYL PKN4766 is a translucent PPO+PS extrusion grade for dilution with polystyrene resin. It is suitable for (microwavable) food packaging and is compliant with US and European food contact regulat.. |
|||
Izod Impact, Notched (ISO) | 1.00 kJ/m² @Temperature 23.0 °C |
0.476 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Noryl PX0346 PPE+PS This data was supplied by SABIC-IP for the Americas region. |