Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ExxonMobil 103 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ExxonMobil 111 Mobilux EP Mobilux EP 111 is an extra high performance grease primarily designed for lubrication of all designs of couplings. It is specifically formulated to resist centrifugal separation of the oil from the .. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ExxonMobil 222 Special Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ExxonMobil 221 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2783 |
ConocoPhillips Syncon® 220 Synthetic EP Gear Oil, AGMA No. 5EP Syncon EP Plus Gear Oil is a premium quality, synthetic, extreme-pressure industrial gear lubricant developed for the lubrication of enclosed gear drives and heavily loaded plain or rolling-element .. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D974 |
ConocoPhillips Syncon® 680 Synthetic EP Gear Oil, AGMA No. 8EP Description: Conoco Syncon Synthetic EP Gear Oil is a synthetic polyalphaolefin (PAO) lubricant for enclosed gear sets requiring extreme-pressure gear oils and operating at high temperatures. It is .. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ConocoPhillips Syncon® Extra Long Life Grease NLGI No. 00 Description: Conoco Syncon Extra Long Life Grease is an ultra high performance lithium-complex grease with heavy synthetic base oil specifically designed for long service life under heavily loaded c.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ConocoPhillips SynXPA® H-500 H Lubricant H-500 Description: Conoco SynXPA H Lubricant is a premium-quality synthetic-polyolester lubricant that offers protection for heavily loaded and partially opened open gears, such as those in ball mills, sh.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ConocoPhillips Tacna® HD Grease NLGI Grade 1 Tacna HD is a premium quality, adhesive, extreme-pressure (EP) lithium complex grease developed for the lubrication of heavily loaded construction, mining and industrial equipment. It also is recomm.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D-2596 |
ConocoPhillips Tacna® M5 Grease NLGI Grade 1 Description: Conoco Tacna M5 Grease is a high-performance, lithium-complex grease with 5% molybdenum disulfide specifically designed for extreme loading conditions. The combination of highly refined.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ChevronTexaco 250 NC-HT Open Gear Lubricant FeaturesChevron Open Gear Lubricants are black, viscous lubricants formulated with an asphaltic base and diluted with a nonchlorinated solvent for easy application by hand or through automatic lubri.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ChevronTexaco 800 NC Open Gear Lubricant FeaturesChevron Open Gear Lubricants are black, viscous lubricants formulated with an asphaltic base and diluted with a nonchlorinated solvent for easy application by hand or through automatic lubri.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ChevronTexaco FM NLGI 1 Grease EP FeaturesChevron FM Greases EP are high performance, multipurpose food machinery greases that are white in color, odorless, tasteless, and water-resistant. Available in three grades, Chevron FM Greas.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ChevronTexaco Multifak® EP NLGI Grade 0 Texaco Multifak EP greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protec.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ChevronTexaco Multifak® EP NLGI Grade 2 Texaco Multifak EP greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protec.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | Weld Point |
ChevronTexaco NLGI 2 Moly Grease EP FeaturesChevron Moly Greases EP are general purpose, extreme pressure (EP) greases. They are manufactured using highly refined selected base oils, a lithium-12-hydroxystearate thickener, 3% molybden.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ChevronTexaco Open Gear Grease FeaturesChevron Open Gear Greases are formulated with high viscosity mineral oils in a nonsoap-based thickener. These greases appear brownish-black and are extremely tacky.Chevron Open Gear Greases .. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | Weld Point |
ChevronTexaco RPM® NLGI 1 Automotive LC Grease EP FeaturesChevron RPM Automotive LC Grease EP is a water resistant, extreme pressure, heavy duty chassis, wheel bearing and general purpose lubricating grease. It is manufactured using highly refined,.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | Weld Point |
ChevronTexaco RPM® NLGI 1 Heavy Duty LC Grease EP FeaturesChevron RPM Heavy Duty LC Greases EP are multipurpose, water resistant, extreme pressure, heavy duty chassis, wheel bearing, and general purpose lubricating greases.They are manufactured usi.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | Weld Point |
ChevronTexaco RPM® NLGI 2 Automotive LC Grease EP FeaturesChevron RPM Automotive LC Grease EP is a water resistant, extreme pressure, heavy duty chassis, wheel bearing and general purpose lubricating grease. It is manufactured using highly refined,.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | Weld Point |
ChevronTexaco RPM® NLGI 2 Heavy Duty LC Grease EP FeaturesChevron RPM Heavy Duty LC Greases EP are multipurpose, water resistant, extreme pressure, heavy duty chassis, wheel bearing, and general purpose lubricating greases.They are manufactured usi.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ChevronTexaco Starplex® Moly MPGM 2 Texaco Starplex Moly MPGM grease delivers value through:Good water resistance — Seals out water, reducing rust and corrosion.Extreme pressure protection.Protection against shock loading, extending .. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ChevronTexaco Starplex® Moly NLGI Grade 1 Texaco Starplex Moly greases deliver value through:Good water resistance — Seals out water, reducing rust and corrosion.Extreme pressure protection.Protection against shock loading — extending veh.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ExxonMobil 221 Mobilgrease FM Mobilgrease FM 221 and FM 222 are high performance multi-purpose products designed specifically for the lubrication of food processing machinery. Mobilgrease FM 221 and FM 222 are formulated with co.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ExxonMobil 222 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | ASTM D2596 |
ExxonMobil Mobilgrease XTC Mobilgrease XTC is an extra high performance product designed for use in high speed coupling applications. It is manufactured with a selected high viscosity mineral base oil and an extremely effecti.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ConocoPhillips IGL-9 Enclosed Gear Lubricant ISO 1000, AGMA Number 8A EP Description: Conoco IGL-9 Enclosed Gear Lubricant is a superior-quality, black, heavy, extreme-pressure gear lubricant developed specifically for enclosed gear sets operating under severe service co.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ConocoPhillips IGL-9 Enclosed Gear Lubricant ISO 680, AGMA Number 8EP Description: Conoco IGL-9 Enclosed Gear Lubricant is a superior-quality, black, heavy, extreme-pressure gear lubricant developed specifically for enclosed gear sets operating under severe service co.. |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ConocoPhillips SUPER-STA M NLGI No.2 Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C... |
|||
Four Ball Extreme Pressure, Weld Load | 315 kg | 695 lb (mass) | |
ConocoPhillips Tacna® 2000 NLGI No. 1 Description: Conoco Tacna 2000 is available in two NLGI grades: No. 1 and No. 2. The No. 2 grade is ideal for use in heavily loaded sleeve-type bushings and bearings subjected to shock loading and o.. |