Izod Impact, Notched (ISO) 11.0 - 12.0 kJ/m²
5.23 - 5.71 ft-lb/in²
ASTM D256
Polikim EFALON® B-40 PTFE, 40% Bronze Filled
Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing..
Izod Impact, Notched (ISO) 2.50 - 12.0 kJ/m²
1.19 - 5.71 ft-lb/in²
Average value: 6.75 kJ/m² Grade Count:6
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are..
Izod Impact, Notched (ISO) 4.30 - 12.0 kJ/m²
2.05 - 5.71 ft-lb/in²
Average value: 8.17 kJ/m² Grade Count:19
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Izod Impact, Notched (ISO) 4.00 - 12.0 kJ/m²

@Temperature -30.0 - -30.0 °C
1.90 - 5.71 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 8.83 kJ/m² Grade Count:10
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
Izod Impact, Notched (ISO) 10.0 - 12.0 kJ/m²

@Temperature -30.0 - -30.0 °C
4.76 - 5.71 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 10.8 kJ/m² Grade Count:5
Overview of materials for Polycarbonate, Gamma Radiation Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum..
Izod Impact, Notched (ISO) 11.0 - 12.0 kJ/m²

@Temperature -30.0 - -30.0 °C
5.23 - 5.71 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 11.7 kJ/m² Grade Count:3
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Izod Impact, Notched (ISO) 2.50 - 12.0 kJ/m²
1.19 - 5.71 ft-lb/in²
Average value: 5.29 kJ/m² Grade Count:33
Overview of materials for Nylon 6, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app..
Izod Impact, Notched (ISO) 3.00 - 12.0 kJ/m²

@Temperature -40.0 - -20.0 °C
1.43 - 5.71 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 5.62 kJ/m² Grade Count:17
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Izod Impact, Notched (ISO) 3.00 - 12.0 kJ/m²
1.43 - 5.71 ft-lb/in²
Average value: 6.00 kJ/m² Grade Count:4
Overview of materials for Nylon 66, 10% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ..
Izod Impact, Notched (ISO) 12.0 - 12.0 kJ/m²

@Temperature -40.0 - -40.0 °C
5.71 - 5.71 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 12.0 kJ/m² Grade Count:1
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an..
Izod Impact, Notched (ISO) 2.00 - 12.0 kJ/m²
0.952 - 5.71 ft-lb/in²
Average value: 4.05 kJ/m² Grade Count:14
Overview of materials for Polypropylene with 40% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are..
Izod Impact, Notched (ISO) 3.80 - 12.0 kJ/m²
1.81 - 5.71 ft-lb/in²
Average value: 6.65 kJ/m² Grade Count:18
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Izod Impact, Notched (ISO) 8.50 - 12.0 kJ/m²
4.04 - 5.71 ft-lb/in²
Average value: 10.2 kJ/m² Grade Count:8
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%