Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 8.50 - 9.00 kJ/m² | 4.04 - 4.28 ft-lb/in² | ASTM D256 |
Polikim EFALON® K-25 PTFE, 25% Carbon Filled K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings... |
|||
Izod Impact, Notched (ISO) | 9.00 - 9.00 kJ/m² @Temperature -30.0 - -30.0 °C |
4.28 - 4.28 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 9.00 kJ/m² Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Izod Impact, Notched (ISO) | 2.60 - 9.00 kJ/m² | 1.24 - 4.28 ft-lb/in² | Average value: 6.18 kJ/m² Grade Count:20 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Izod Impact, Notched (ISO) | 6.00 - 9.00 kJ/m² @Temperature -30.0 - -30.0 °C |
2.86 - 4.28 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 7.50 kJ/m² Grade Count:2 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Izod Impact, Notched (ISO) | 6.00 - 9.00 kJ/m² | 2.86 - 4.28 ft-lb/in² | Average value: 7.00 kJ/m² Grade Count:3 |
Overview of materials for Acetal Copolymer, Silicone Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched (ISO) | 5.00 - 9.00 kJ/m² @Temperature -30.0 - -30.0 °C |
2.38 - 4.28 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 7.80 kJ/m² Grade Count:5 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Izod Impact, Notched (ISO) | 8.00 - 9.00 kJ/m² @Temperature -30.0 - -30.0 °C |
3.81 - 4.28 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 8.50 kJ/m² Grade Count:2 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%.. |
|||
Izod Impact, Notched (ISO) | 6.00 - 9.00 kJ/m² @Temperature -40.0 - -30.0 °C |
2.86 - 4.28 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 7.55 kJ/m² Grade Count:11 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |
|||
Izod Impact, Notched (ISO) | 9.00 - 9.00 kJ/m² @Temperature -30.0 - -30.0 °C |
4.28 - 4.28 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 9.00 kJ/m² Grade Count:2 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |
|||
Izod Impact, Notched (ISO) | 4.98 - 9.00 kJ/m² @Temperature -40.0 - -20.0 °C |
2.37 - 4.28 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 7.24 kJ/m² Grade Count:4 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |