Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 7.30 - 30.0 kJ/m² | 3.47 - 14.3 ft-lb/in² | Average value: 13.3 kJ/m² Grade Count:9 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Izod Impact, Notched (ISO) | 9.00 - 30.0 kJ/m² | 4.28 - 14.3 ft-lb/in² | Average value: 13.7 kJ/m² Grade Count:6 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%.. |
|||
Izod Impact, Notched (ISO) | 11.0 - 30.0 kJ/m² | 5.23 - 14.3 ft-lb/in² | Average value: 15.9 kJ/m² Grade Count:5 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Izod Impact, Notched (ISO) | 2.94 - 30.0 kJ/m² | 1.40 - 14.3 ft-lb/in² | Average value: 15.1 kJ/m² Grade Count:17 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |