Polymer Property : Izod Impact, Notched (ISO) = 13.3 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 9.00 - 28.0 kJ/m²
4.28 - 13.3 ft-lb/in²
Average value: 16.6 kJ/m² Grade Count:18
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Izod Impact, Notched (ISO) 4.00 - 28.0 kJ/m²
1.90 - 13.3 ft-lb/in²
Average value: 15.2 kJ/m² Grade Count:31
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi..
Izod Impact, Notched (ISO) 2.40 - 28.0 kJ/m²
1.14 - 13.3 ft-lb/in²
Average value: 8.43 kJ/m² Grade Count:14
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
Izod Impact, Notched (ISO) 16.0 - 28.0 kJ/m²
7.61 - 13.3 ft-lb/in²
Average value: 20.7 kJ/m² Grade Count:6
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum..