Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.40 kJ/m² | 1.62 ft-lb/in² | ISO 180/1eA |
Polyplastic Armlen® PP MF 20-2HS-901 Polypropylene, 20% Mineral Filled Heat stabilized, black colored, HVAC applicationsInformation provided by PolyPlastic Group. |
|||
Izod Impact, Notched (ISO) | 3.40 kJ/m² @Temperature 23.0 °C |
1.62 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Qualchem Danamid FEWLX2-25 Polyamide 6, 25% Mineral Filled Filled with minerals. Flame retardant, halogen-free (V-2)Information provided by Qualchem Zrt. |
|||
Izod Impact, Notched (ISO) | 3.40 kJ/m² | 1.62 ft-lb/in² | ISO 180/1A |
Lucite International Diakon® ST25G6 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Izod Impact, Notched (ISO) | 3.40 kJ/m² | 1.62 ft-lb/in² | ISO 180/1A |
Lucite International Diakon® ST25G7 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Izod Impact, Notched (ISO) | 3.40 kJ/m² | 1.62 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® MR410 22H-GY1 40% Mineral Reinforced Nylon 66 Description: Mineral Reinforced Nylon 66Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 3.40 kJ/m² @Temperature -40.0 °C |
1.62 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A |
DuPont Performance Polymers Minlon® 22C BK086 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C BK086 is a 38% mineral/glass reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performance.. |
|||
Izod Impact, Notched (ISO) | 3.40 kJ/m² | 1.62 ft-lb/in² | ISO 180/1A |
A.D. Compound Adene NCJA Homopolymer 30% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Izod Impact, Notched (ISO) | 3.40 - 14.0 kJ/m² | 1.62 - 6.66 ft-lb/in² | Average value: 6.40 kJ/m² Grade Count:4 |
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |