Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 11.5 kJ/m²
5.47 ft-lb/in²
ISO 180
Polycasa PETG
QUINN PETG has good optical properties and a brilliant surface. The PETG range of sheets are easy to fabricate, to vacuum form, and show exceptional low temperature performance. Important benefits o..
Izod Impact, Notched (ISO) 11.5 kJ/m²

@Temperature 23.0 °C
5.47 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac..
Izod Impact, Notched (ISO) 11.5 kJ/m²
5.47 ft-lb/in²
ISO 180-1A
Gromax BFG30-AS00N1 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Izod Impact, Notched (ISO) 11.5 kJ/m²
5.47 ft-lb/in²
GB/T 1843-2008
Sichuan Deyang Haton® hGR302 PPS / F4 Polyphenylene Sulfide
Injection molding, anti-frictionInformation provided by Sichuan Deyang Chemical Co., LTD
Izod Impact, Notched (ISO) 11.5 kJ/m²
5.47 ft-lb/in²
ISO 180
Polyram PlusTek PA4501G6 Nylon 66, 30% Glass Fiber Reinforced, Low Friction
30% Glass fiber reinforced Nylon 66 for low friction applications.Information provided by Polyram.
Izod Impact, Notched (ISO) 11.5 kJ/m²
5.47 ft-lb/in²
ASTM D256
Total PSI 3341 High Impact Polystyrene
Total Petrochemicals Polystyrene 3341 is a high impact polystyrene for the extrusion industry. Its good mechanical and thermal properties leads to the production of thermoformed articles of good ri..
Izod Impact, Notched (ISO) 11.5 kJ/m²

@Temperature -40.0 °C
5.47 ft-lb/in²

@Temperature -40.0 °F
ISO Test
BASF Petra® 140 BK-112 45% Glass Filled PET
Petra 140 BK-112 is a 45% glass reinforced, pigmented black, polyethylene terephthalate (PET) injection molding compound offering an increased level of strength, stiffness, high temperature performa..
Izod Impact, Notched (ISO) 11.5 kJ/m²
5.47 ft-lb/in²
ISO 180/A
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Dry)
Ultramid A3EG6 is a 30% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability.
Izod Impact, Notched (ISO) 11.5 - 11.5 kJ/m²

@Temperature -40.0 - -40.0 °C
5.47 - 5.47 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 11.5 kJ/m² Grade Count:1
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Copyright © lookpolymers.com All Rights Reserved