Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 23.0 - 55.0 kJ/m²
10.9 - 26.2 ft-lb/in²
Average value: 42.3 kJ/m² Grade Count:6
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Izod Impact, Unnotched (ISO) 40.0 - 55.0 kJ/m²

@Temperature -30.0 - -30.0 °C
19.0 - 26.2 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 47.5 kJ/m² Grade Count:2
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Izod Impact, Unnotched (ISO) 25.0 - 55.0 kJ/m²
11.9 - 26.2 ft-lb/in²
Average value: 40.2 kJ/m² Grade Count:6
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
Izod Impact, Unnotched (ISO) 15.0 - 55.0 kJ/m²
7.14 - 26.2 ft-lb/in²
Average value: 31.3 kJ/m² Grade Count:4
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
Izod Impact, Unnotched (ISO) 20.0 - 55.0 kJ/m²
9.52 - 26.2 ft-lb/in²
Average value: 28.3 kJ/m² Grade Count:11
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Izod Impact, Unnotched (ISO) 30.0 - 55.0 kJ/m²
14.3 - 26.2 ft-lb/in²
Average value: 39.4 kJ/m² Grade Count:9
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
Izod Impact, Unnotched (ISO) 28.0 - 55.0 kJ/m²
13.3 - 26.2 ft-lb/in²
Average value: 42.2 kJ/m² Grade Count:9
Overview of materials for Polypropylene with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i..
Izod Impact, Unnotched (ISO) 17.0 - 55.0 kJ/m²
8.09 - 26.2 ft-lb/in²
Average value: 37.3 kJ/m² Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported..