Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 120 kJ/m² | 57.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP COLORCOMP D1000 PC (Europe-Africa-Middle East) LNP* COLORCOMP* D1000 is a compound based on Polycarbonate resin containing Unfilled Custom Color |
|||
Izod Impact, Unnotched (ISO) | 120 kJ/m² | 57.1 ft-lb/in² | ISO 180 |
LNP Lubricomp® FL-4410 Polyetherimide, Silicone Lubricant Additive
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Izod Impact, Unnotched (ISO) | 120 kJ/m² @Temperature 23.0 °C |
57.1 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon DD0009XQ PC (Europe-Africa-Middle East) LNP* Stat-Kon* DD0009XQ is a compound based on Polycarbonate containing Carbon Powder and Flame Retardant. Added features include Electrically Conductive, Flame Retardant and Easy Molding.This data.. |
|||
Izod Impact, Unnotched (ISO) | 120 kJ/m² | 57.1 ft-lb/in² | |
Shandong Guangyin 1212 Reinforced Nylon Features and Applications: Wear resistance, higher strength, better tenacity, strong adhesion and better low temperature resistance. It is applicable to surface coating of wires, cables, optical cab.. |
|||
Izod Impact, Unnotched (ISO) | 120 kJ/m² | 57.1 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Star L POM D11 POM, Injection Molded Star L POM D11 is Silicone Oil Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |