Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 5.10 J/cm² @Temperature 23.0 °C |
24.3 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PH 49 GF 30 TS PP, 30% glass fibre, mod. of mech. Properties FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Charpy Impact Unnotched | 5.10 J/cm² @Temperature 23.0 °C |
24.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPH GF5020 HC Polypropylene Homopolymer, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Charpy Impact Unnotched | 5.10 J/cm² @Temperature -30.0 °C |
24.3 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radiflam® A RV300AF (cond.) Nylon 66-30GF Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g.. |
|||
Charpy Impact Unnotched | 5.10 J/cm² @Temperature -20.0 °C |
24.3 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GF 15 HI PA6, 15% glass fibre, improved strength FeaturesPA 6 for injection moulding, chemically strengthened with 15% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and.. |
|||
Charpy Impact Unnotched | 5.10 J/cm² @Temperature -30.0 °C |
24.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Charpy Impact Unnotched | 5.10 J/cm² @Temperature -30.0 °C |
24.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Charpy Impact Unnotched | 5.10 J/cm² @Temperature 23.0 °C |
24.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Sax Polymers SAXAMID 226F4 Nylon 6.6, 20% Glass Fiber SAXAMID 226F4 is a polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers.Information provided by SAX Polymers |
|||
Charpy Impact Unnotched | 5.10 J/cm² @Temperature 23.0 °C |
24.3 ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact Unnotched | 5.10 J/cm² @Temperature 23.0 °C |
24.3 ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Asia Pacific) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Charpy Impact Unnotched | 5.10 J/cm² @Temperature 23.0 °C |
24.3 ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Europe-Africa-Middle East) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact Unnotched | 5.10 J/cm² @Temperature -30.0 °C |
24.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact Unnotched | 5.10 J/cm² @Temperature 23.0 °C |
24.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1fU |
Borealis Nepol™ GB601HP Polypropylene, 40% Long Glass Fiber Reinforced w/BJ356MO Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Charpy Impact Unnotched | 5.10 J/cm² @Temperature 23.0 °C |
24.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R633 Nylon 66 Copolymer, 33% Glass Filled, Dry as Molded Vydyne® R633 is 33% glass-fiber reinforced, PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold .. |
|||
Charpy Impact Unnotched | 5.10 J/cm² @Temperature 23.0 °C |
24.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Ascend Performance Materials Vydyne® R633H Nylon 66/6, 33% Glass Reinforced, DAM Vydyne® R633H is 33% glass-fiber reinforced PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold .. |
|||
Charpy Impact Unnotched | 5.10 J/cm² @Temperature 23.0 °C |
24.3 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PH 69 GF 40 PP, 40% glass fibre, mod. of mech. properties FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 40% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |