Polymer Property : Charpy Impact Unnotched = 109 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 23.0 J/cm²

@Temperature -30.0 °C
109 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Lanxess Pocan® B 1700 000000 PBT
PBT, non-reinforced, extrusion, food contact
Charpy Impact Unnotched 23.0 J/cm²

@Temperature -30.0 °C
109 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® 500PE NC010A Acetal Homopolymer
Delrin® 500PE NC010A is a medium viscosity acetal homopolymer, an enhanced version of Delrin® 500P with extremely low VOC emissions. It has improved processing thermal stability, and good mechanic..
Charpy Impact Unnotched 23.0 J/cm²

@Temperature 23.0 °C
109 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
BASF Ultraform® E 3120 BM POM
Description: Is a POM, high-molecular grade for extrusion blow molding of hollow parts.Information provided by BASF
Charpy Impact Unnotched 23.0 J/cm²

@Temperature -30.0 °C
109 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultraform® N2640 Z2 POM + PUR
Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS..
Charpy Impact Unnotched 23.0 J/cm²

@Temperature -30.0 °C
109 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultraform® N2320 0035 POM
Description: Rapidly solidifying standard grade for injection molding.Information provided by BASF