Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 3.40 J/cm² @Temperature -20.0 °C |
16.2 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 99 GB 30 LS PP, 30% glass beads, mod. of mech. properties FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Charpy Impact Unnotched | 3.40 J/cm² @Temperature -30.0 °C |
16.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
PolyOne OnFlex™ BIO 5180D-E0014 Thermoplastic Elastomer (TPE) OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab.. |
|||
Charpy Impact Unnotched | 3.40 J/cm² @Temperature 23.0 °C |
16.2 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
Qualchem Danamid FGFLX2-30 Polyamide 6, 30% Glass Fiber Reinforced with glass fiber. Flame retardant, halogen-free (V-2)Information provided by Qualchem Zrt. |
|||
Charpy Impact Unnotched | 3.40 J/cm² @Temperature 23.0 °C |
16.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Sax Polymers SAXAMID 126K6 Nylon 6, 30% Glass Filled SAXAMID 126K6 is a 30% glass beads filled polyamide 6 injection-molding-grade. It is characterized by dimensional stability, low warpage and good surface quality.Information provided by SAX Polymers.. |
|||
Charpy Impact Unnotched | 3.40 J/cm² @Temperature 23.0 °C |
16.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Sax Polymers SAXAMID 226K6 Nylon 6.6, 30% Glass Beads SAXAMID 226K6 is a polyamide 6.6 injection-molding-grade filled with 30% glass beads. It is characterized by optimized shrinkage properties.Information provided by SAX Polymers |
|||
Charpy Impact Unnotched | 3.40 J/cm² @Temperature -30.0 °C |
16.2 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® VX4015 PBT (Europe-Africa-Middle East) VALOX VX4015 is a 15% glass reinforced PBT injection moulding resin, with excellent hydrolytical stability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact Unnotched | 3.40 J/cm² @Temperature 23.0 °C |
16.2 ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® VX5530 PBT (Europe-Africa-Middle East) VALOX VX5530 is a flame retarded, 15% glass fibre reinforced, 10% mineral filled PBT+PC blend with excellent low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Charpy Impact Unnotched | 3.40 J/cm² @Temperature -30.0 °C |
16.2 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® VX5530 PBT (Europe-Africa-Middle East) VALOX VX5530 is a flame retarded, 15% glass fibre reinforced, 10% mineral filled PBT+PC blend with excellent low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |