Polymer Property : Tensile Strength at Break = 4350 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.0 - 30.0 MPa
2900 - 4350 psi
ASTM D638-03
Proto3000 Objet DurusWhite FullCure430 Polypropylene-like Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
Tensile Strength at Break 28.0 - 30.0 MPa
4060 - 4350 psi
ASTM D683
Loxim 830 02T HB Polypropylene Compound, 30% Talc Filled, Flame Retardant
Information provided by Loxim Industries
Tensile Strength at Break 14.0 - 30.0 MPa

@Thickness 2.00 mm
2030 - 4350 psi

@Thickness 0.0787 in
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)
Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional ..
Tensile Strength at Break 14.0 - 30.0 MPa

@Thickness 2.00 mm
2030 - 4350 psi

@Thickness 0.0787 in
50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 32008 Polyvinylidene Fluoride (PVDF)
Solef® 32008 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional ..
Tensile Strength at Break 20.0 - 30.0 MPa
2900 - 4350 psi
ZCI-T-008
Zeon Chemicals Zetpol® 2020 Hydrogenated Nitrile Elastomomer
Zetpol 2020 is a highly saturated copolymer of butadiene and acrylonitrile with high tensile strength, good heat resistance, good chemical resistance to aggressive fluids, and an excellent balance o..
Tensile Strength at Break 20.0 - 30.0 MPa
2900 - 4350 psi
ZCI-T-008
Zeon Chemicals Zetpol® 2020L Hydrogenated Nitrile Elastomomer
Zetpol 2020L is a highly saturated copolymer of butadiene and acrylonitrile with high tensile strength, good heat resistance, good chemical resistance to aggressive fluids, and an excellent balance ..
Tensile Strength at Break 15.0 - 30.0 MPa
2180 - 4350 psi
TM-019G
AorTech Biomaterials Elast-Eon™ E5-325 Biomedical Polyurethane Pellets
Elast-Eon™ 5-325 is a polyurethane with a 32.5% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in ..
Tensile Strength at Break 15.0 - 30.0 MPa
2180 - 4350 psi
TM-019G
AorTech Biomaterials Elast-Eon™ E5-325 Biomedical Polyurethane Pellets
Elast-Eon™ 5-325 is a polyurethane with a 32.5% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in ..
Tensile Strength at Break 14.0 - 30.0 MPa

@Thickness 2.00 mm,
Temperature 23.0 °C
2030 - 4350 psi

@Thickness 0.0787 in,
Temperature 73.4 °F
Type IV, 50 mm/min; ASTM D638
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Information provided by Solvay Specialty Polymers.