Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zeon Chemicals Zetpol® 2020L Hydrogenated Nitrile Elastomomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Zetpol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Zetpol® 2020L Hydrogenated Nitrile Elastomomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Zetpol 2020L is a highly saturated copolymer of butadiene and acrylonitrile with high tensile strength, good heat resistance, good chemical resistance to aggressive fluids, and an excellent balance of properties over a wide variation of temperatures.Low Mooney version of Zetpol 2020. Excellent for transfer or injection molding. FDA approved.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
Iodine Absorption Number 23.2 - 32.8
23.2 - 32.8
mg/100mg; ZCI-T-004
Mooney Viscosity 50 - 65

@Temperature 100 °C
50 - 65

@Temperature 212 °F
(1+4); ZCI-T-003
Ash <= 0.50 %
<= 0.50 %
ZCI-T-005
Mechanical Properties Metric English Comments
Hardness, Shore A 67 - 75
67 - 75
ZCI-T-009
Tensile Strength at Break 20.0 - 30.0 MPa
2900 - 4350 psi
ZCI-T-008
Elongation at Break 430 - 530 %
430 - 530 %
ZCI-T-008
300% Modulus 0.01060 - 0.01460 GPa
1.537 - 2.117 ksi
ZCI-T-008
Descriptive Properties Value Comments
% HYD 91
Bound ACN (%, acrylonitrile) 34.9-37.5
Heat Loss (%) Max 0.5
Users viewing this material also viewed the following: