Mechanical Properties Metric English Comments
Tensile Strength at Break 320 MPa
46400 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP LC00APXQ PEEK
LNP* THERMOCOMP* LC00APXQ is a compound based on Polyetheretherketone resin containing 50% Carbon Fiber. Added features of this material include: Exceptional Processing, Electrically Conductive.
Tensile Strength at Break 320 - 740 MPa
46400 - 107000 psi
Goodfellow Phosphor Bronze
Good Machinability. Uses include springs, clips, gauzes and architectural applicationsInformation provided by Goodfellow.
Tensile Strength at Break 320 - 620 MPa
46400 - 89900 psi
Goodfellow Platinum 90/Rhodium 10 Thermocouple Alloy
The positive element of the type S thermocouple. Type S thermocouples are characterized by a high degree of chemical inertness and stability at high temperatures. Often used as a standard for calibr..