Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 29.2 MPa | 4230 psi | ASTM D638 |
Westlake Plastics Propylux® 290 Polypropylene, Heat Stabilized Through process improvement and advanced engineering, Westlake Plastics introduces the next generation of heat-stabilized polypropylene. Propylux 290 is produced from a FDA approved homopolymer res.. |
|||
Tensile Strength at Break | 29.2 MPa | 4230 psi | ASTM D638 |
Westlake Plastics Propylux® HS2 Polypropylene for Medical Applications, Heat Stabilized Through process improvement and advanced engineering, Westlake Plastics introduces the next generation of heat-stabilized polypropylene. Propylux HS2 is produced from a FDA and USP Class VI approve.. |
|||
Tensile Strength at Break | 29.2 MPa | 4230 psi | ASTM D3756 |
3M 203 Masking Tape 3M™ Masking Tape 203 is a general purpose masking tape that can be used for holding, bundling, sealing and a vast number of other jobs where a pressure- sensitive tape is needed.Information provide.. |