Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 20.7 MPa | 3000 psi | 2 in/min; ASTM D638 |
RheTech Products HP521-00 15% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 20.7 MPa | 3000 psi | 2 in/min; ASTM D638 |
RheTech Products HP521-01 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 20.7 MPa | 3000 psi | 2 in/min; ASTM D638 |
RheTech Products HP521-231 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 173B Navy Blue Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 20.7 MPa | 3000 psi | UL 1581 |
PolyOne OnFlex™ HFFR 310-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 310-01 is a non-halogen flame retardant material designed for cable jackets. New Product. Commercial specifications have not been established. - Non-halogen flame retardant - UL62 comp.. |
|||
Tensile Strength at Break | 20.7 MPa | 3000 psi | UL 1581 |
PolyOne OnFlex™ HFFR 315-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 315-01 a is non-halogen flame retardant material designed for flexible power cord insulation, cable jackets, and ribbon cables. New Product. Commercial specifications have not been est.. |
|||
Tensile Strength at Break | 20.7 MPa | 3000 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A4D02 Polyvinyl Chloride, Flexible (PVC, Flexible) A flexible transparent PVC Compound designed primarily for indoor mats.Information provided by PolyOne |
|||
Tensile Strength at Break | 20.7 MPa | 3000 psi | ASTM D638 |
Resirene Resirene® 6420 Super High Impact Polystyrene Features:Super High ImpactEasy ProcessingLow ModulusFlexibilityFDA Rating: 21 CFR 177.1640Applications:ExtrusionDeep ThermoformingGPPS/HIPS BlendsPoint of Purchase DisplaysInformation provided by US.. |
|||
Tensile Strength at Break | 20.7 MPa | 3000 psi | 2 in/min; ASTM D638 |
RheTech Products HP522-286 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, ZUCA Medium Graphite Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 20.7 MPa | 3000 psi | 2 in/min; ASTM D638 |
RheTech Products HP522-473 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, ZU5A Dark Graphite Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 20.7 MPa | 3000 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible G92C Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 20.7 MPa | 3000 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R1480E Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength at Break | 20.7 MPa | 3000 psi | AVG; ASTM D412 Method A |
Seals Eastern 7130 Fluorocarbon-Elastomer FKM specially for oil & gas service.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength at Break | 20.7 MPa | 3000 psi | ASTM D638 |
Teknor Apex APEX® 6500-105 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Extrusion Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molded Compon.. |
|||
Tensile Strength at Break | 20.7 MPa | 3000 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Tensile Strength at Break | 20.7 MPa | 3000 psi | ASTM D412 |
Teknor Apex Telcar® TL-1000-105UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 20.7 MPa | 3000 psi | at max load; ASTM D638 |
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Tensile Strength at Break | 20.7 MPa | 3000 psi | at max load; ASTM D638 |
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Tensile Strength at Break | 20.7 MPa | 3000 psi | ASTM C370 |
Chesterton ARC 988 Composite Description: A high performance, quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by severe chemical and physi.. |
|||
Tensile Strength at Break | 20.7 MPa | 3000 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 203-40 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Tensile Strength at Break | 20.7 MPa | 3000 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Tensile Strength at Break | 20.7 - 24.1 MPa | 3000 - 3500 psi | TM R050-36 |
Resinlab® EP1305LV Black Epoxy Casting Resin Resinlab™ EP1305LV Black is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c.. |
|||
Tensile Strength at Break | 20.7 - 24.1 MPa | 3000 - 3500 psi | TM R050-36 |
Resinlab® EP1305LV Clear Epoxy Casting Resin Resinlab™ EP1305LV Clear is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c.. |