Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 17.2 MPa | 2500 psi | 2 in/min; ASTM D638 |
RheTech Products FT1055-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | 2 in/min; ASTM D638 |
RheTech Products FT1055-50 Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | 2 in/min; ASTM D638 |
RheTech Products FT1055-624 Thermoplastic Polyolefin, Non-UV Stabilized, General Purpose Light Grey Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | 2 in/min; ASTM D638 |
RheTech Products FT1055-685UV Thermoplastic Polyolefin, UV Stabilized, Graphite Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | 2 in/min; ASTM D638 |
RheTech Products FT7013-721UV Thermoplastic Polyolefin, UV Stabilized, XDV Dark Slate Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | 2 in/min; ASTM D638 |
RheTech Products FT7016-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | 2 in/min; ASTM D638 |
RheTech Products HP800-706UV 20% Talc Reinforced High Performance Polypropylene Copolymer, Scratch Resistant, UV Stabilized, Impact Modified, SWB White Applications: Interior trim/Instrument panel componentsA/B pillarsGlove box doorsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | chs 20 in; ASTM D412 |
Network Polymers Softflex® 1104 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | Cured |
Resin Technology Group MX-2212 High Impact, Multi-Functional, UV Curing Adhesive This multi-functional product is a rapid setting structural adhesive. UV-MX 2212 provides high impact, resilient bonds to many similar and dissimilar substrates. Multi-functional cure bonds are form.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D4745 |
3M Dyneon™ CC105 Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of 25% fiberglass blended with PTFEInformation provided by Dyneon, A 3M Company |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
LyondellBasell Hifaxâ„¢ RTA3263/2 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ RTA3263/2 medium melt flow, 1,700 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good combination of rigidity, impac.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
Teknor Apex APEX® 121 Polyvinyl Chloride, Flexible Notes: 90°C Jacket; RoHS Compliant Features: Good UV Resistance Uses: Telephone Drop Wire Insulation; Telephone Drop Wire JacketingAgency Ratings: REA Unspecified Rating Forms: PelletsInformation.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
Teknor Apex APEX® 3700-75NT1 Polyvinyl Chloride, Flexible Features: DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
Teknor Apex APEX® 77-W115-B Polyvinyl Chloride, Flexible Notes: 105°C General Purpose; RoHS Compliant Uses: Connects; Grommets; Plugs; Strain ReliefsForms: Pellets Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molded Components Additional Information: T.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D412 |
Teknor Apex Monprene® MP-1287A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D412 |
Teknor Apex Telcar® CR-92-E2555A-92 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D412 |
Teknor Apex Telcar® TL-1472A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
ExxonMobil LLDPE LL 1002YB Wire & Cable Linear Low Density Polyethylene Resin Product Description: LL 1002YB is a C4 Ziegler Natta LLDPE for Low Voltage power cable and Telecom jacketing. The grade contains a higher level of antioxidants and has excellent Environmental Stress.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | |
Abatron WoodEpox® Wood Replacement Compound WoodEpox® is a shrink-free adhesive putty wood replacement compound that can be used in any thickness in structural and decorative applications to replace, repair, extend, or fill wood and material.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D4745 |
3M Dyneon™ CC605 Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of 25% fiberglass blended with PTFE.Information provided by Dyneon, A 3M Company |