Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 17.1 MPa | 2480 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R343AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 17.1 MPa | 2480 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible G8024 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 17.1 MPa | 2480 psi | Press cure 15 Minutes @ 188°C, Post Cure 16 Hours @ 250°C |
3M Dyneon™ PFE 4131TZ High Temperature Perfluoroelastomer 3M™ Dyneon™ PFE 4131TZ is an incorporated cure high temperature perfluoroelastomer (HT PFE). It is designed to meet the challenges of higher temperature applications. It is classified as FFKM per .. |