Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 9.93 MPa | 1440 psi | |
NEU NeuSoft™ 455-60A Ester/ether TPU / SBC blend |
|||
Tensile Strength at Break | 9.93 MPa | 1440 psi | Across Flow; ASTM D412 |
ExxonMobil Vyram™ 9101-85 Thermoplastic Elastomer
(discontinued **) A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Tensile Strength at Break | 9.93 MPa | 1440 psi | Across Flow; ASTM D412 |
ExxonMobil Vyram™ 9201-85 Thermoplastic Elastomer
(discontinued **) A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Tensile Strength at Break | 9.96 MPa | 1440 psi | After 72hr/177°C air oven, ASTM D573 |
DuPont Elvax® 40L-03 High Temperature Ignition Cable Jacket Formulation
(discontinued **) Elvax® 40L-03 high temperature ignition cable jacket.Information provided by DuPont. |
|||
Tensile Strength at Break | 9.93 MPa | 1440 psi | |
Shin-Etsu Silicones SV-17500U Silicone Rubber SV17500U is one of a series of easy processing, silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendaring. Product Features: This pr.. |
|||
Tensile Strength at Break | 9.90 MPa | 1440 psi | after aging 7 days @ 136°C |
Borealis LE0151 Easy Strippable Semiconductive Insulation Shield for Medium Voltage Power Cables LE0515 is an easy strippable crosslinkable semi conductive insulation shield compound designed for medium voltage (5kV-46kV) power cable applications. Application: LE0515 is especially suitable for.. |
|||
Tensile Strength at Break | 9.90 MPa | 1440 psi | ISO 527-1 |
Barlog Plastics KEBAFLEX SG 85 A.01 black TPE-S, Shore A85, black TPE-SInformation provided by BARLOG plastics GmbH. |