Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 8.50 MPa | 1230 psi | ISO 37 |
PolyOne OnFlex™ S FR 80A-3S1892 Thermoplastic Elastomer (TPE) OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo.. |
|||
Tensile Strength at Break | 8.50 MPa | 1230 psi | ASTM D638 |
Petroquimica Triunfo Trithene® CX 7065 LDPE - Extrusion Coating The Trithene® CX 7065 resin is a product developed especially to meet the segment of extrusion coating where the following properties are necessary: processing stability at high production rates, a.. |
|||
Tensile Strength at Break | 8.50 MPa | 1230 psi | ASTM D638 |
Petroquimica Triunfo Trithene® JX 7065 LDPE - Injection Molding and Master Batch The Trithene® JX 7065 resin is a low-density polyethylene with a wide molecular weight distribution, developed to offer good impact resistance, excellent flexibility, and high resistance to stress .. |
|||
Tensile Strength at Break | 8.48 MPa | 1230 psi | Across flow; ASTM D412 |
ExxonMobil Santoprene® 201-73W228 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic elastomer with good fluid resistance, formulated to replace foamed thermoset elastomers such as EPDM and thermoplastic foams. It is polyolefin-based and desig.. |
|||
Tensile Strength at Break | 8.48 MPa | 1230 psi | Crosshead Speed - 20 in/min; ASTM D638 |
LyondellBasell Petrothene® NA860008 Low Density Polyethylene ApplicationsPETROTHENE NA 860 is a series of medium flow, low density polyethylene resins for the injection molding of caps, closures and other specialty applications. These resins exhibit an excel.. |
|||
Tensile Strength at Break | 8.48 MPa | 1230 psi | Crosshead Speed - 20 in/min; ASTM D638 |
LyondellBasell Petrothene® NA860241 Low Density Polyethylene ApplicationsPETROTHENE NA 860 is a series of medium flow, low density polyethylene resins for the injection molding of caps, closures and other specialty applications. These resins exhibit an excel.. |
|||
Tensile Strength at Break | 8.48 MPa | 1230 psi | ASTM D412 |
Teknor Apex Monprene® MP-1852A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.50 MPa | 1230 psi | ASTM D638 |
UBE J3519 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Tensile Strength at Break | 8.48 MPa | 1230 psi | ASTM D412 |
Teknor Apex Telcar® TL-2585A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 8.48 MPa | 1230 psi | ASTM D412 |
Teknor Apex Telcar® TL-2585F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 8.48 MPa | 1230 psi | ASTM D 412 |
CPT C-Flex® R70-003 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Tensile Strength at Break | 8.50 MPa | 1230 psi | ISO 37 |
ELASTO UK Dryflex® 3031-102 TPE, Modified Injection Molding Grade for Auto Interior Parts The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3031-102 is specifically designe.. |
|||
Tensile Strength at Break | 8.48 MPa | 1230 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8223-30M300 Thermoplastic Elastomer A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and .. |
|||
Tensile Strength at Break | 8.50 MPa | 1230 psi | ISO 527-1 |
Barlog Plastics KEBAFLEX SG 75 A.1 black TPE-S, Shore A75, black TPE-SInformation provided by BARLOG plastics GmbH. |
|||
Tensile Strength at Break | 8.50 MPa | 1230 psi | ISO 527-1 |
Barlog Plastics KEBAFLEX SG 75 A.1 TPE-S, Shore A70, natural TPE-SInformation provided by BARLOG plastics GmbH. |
|||
Tensile Strength at Break | 8.48 MPa | 1230 psi | ISO 37 |
Alliance Polymers Viprene™ G75A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G75A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 8.48 MPa | 1230 psi | ISO 37 |
Alliance Polymers Viprene™ G75A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G75A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 8.48 MPa | 1230 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 201-73W175 Thermoplastic Elastomer
(discontinued **) A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for thin wall .. |