Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 8.83 MPa @Temperature 23.0 °C |
1280 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne OnFlex™ HFFR 360-0185 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 360-0185 is a non-halogen flame retardant material designed for injection molding applications. New Product. Commercial specifications have not been established. - Non-halogen flame re.. |
|||
Tensile Strength at Break | 8.83 MPa | 1280 psi | chs 20 in/min; ASTM D412 |
Network Polymers Softflex® 5000 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tensile Strength at Break | 8.83 MPa | 1280 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 221-73 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Tensile Strength at Break | 8.83 MPa | 1280 psi | ASTM D638 |
Lotte Chemical Titan TITANEX® LI2516 Linear low density polyethylene resin
(discontinued **) LI2516 is a pelleted linear low density polyethylene with very narrow molecular weight distribution.Applications: House-wares, lids, closures and toys.Advantages: Excellent stress crack resistance,.. |
|||
Tensile Strength at Break | 8.83 MPa | 1280 psi | |
Shin-Etsu Silicones KE-9510U Silicone Elastomer KE9510 U is one of a series of easy processing, general purpose silicone rubber base with low volatile content. It can be used in a variety of applications requiring finishing by molding, extruding .. |
|||
Tensile Strength at Break | 8.83 MPa | 1280 psi | |
Shin-Etsu Silicones FEA-271U Fluorosilicone Elastomer ShinEtsu FEA271 U is one of a series of fluorosilicone compounds. It is designed to process well in molding applications. It can be blended with other members of the series for intermediate hardness.. |
|||
Tensile Strength at Break | 8.83 MPa | 1280 psi | |
Shin-Etsu Silicones KE-5530U Low Temperature Silicone Elastomer ShinEtsu KE5530 U is a nominal 30 Durometer phenyl (PVMQ) base.Product Features: This material was designed for its excellent vibration dampening characteristics. Because of its phenyl content, it a.. |
|||
Tensile Strength at Break | 8.83 MPa | 1280 psi | |
Shin-Etsu Silicones KE-951U Silicone Elastomer KE951 U is one of a series of easy processing, general purpose silicone rubber bases. It can be used in a variety of applications requiring finishing by molding (compression, injection, transfer).Pr.. |
|||
Tensile Strength at Break | 8.83 MPa | 1280 psi | ASTM D412 |
Teknor Apex Monprene® MP-1383B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.83 MPa | 1280 psi | 20 in/min; ASTM D412 |
Teknor Apex Telcar® TL-1140D BLK Thermoplastic Elastomer Uses: Automotive Applications; Automotive Interior Parts; Blow Molding Applications; Carpet Backing; General Purpose; Grommets; Weatherstripping Forms: Pellets Processing Method: Extrusion; Injectio.. |
|||
Tensile Strength at Break | 8.83 MPa | 1280 psi | ASTM D412 |
Teknor Apex Telcar® TL-2580F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 8.83 MPa | 1280 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 121-73W175 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for .. |
|||
Tensile Strength at Break | 8.83 MPa | 1280 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 201-73 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Tensile Strength at Break | 8.83 MPa | 1280 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 241-73W236 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and contains.. |
|||
Tensile Strength at Break | 8.83 MPa | 1280 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 171-73 Thermoplastic Elastomer A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Tensile Strength at Break | 8.83 MPa | 1280 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 271-73 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Tensile Strength at Break | 8.83 MPa | 1280 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 241-73 Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Tensile Strength at Break | 8.83 MPa | 1280 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 101-73 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |