Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 77.9 MPa | 11300 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ 1280 A HS Black 11 A Polyamide 66 (Nylon 66) The Nymax® 1200 Blend Series of nylon 6/6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materi.. |
|||
Tensile Strength at Break | 77.9 MPa | 11300 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ 600 A HS Natural A Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Tensile Strength at Break | 77.9 MPa | 11300 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ 600 A Natural 12 Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Tensile Strength at Break | 77.9 MPa | 11300 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ 600 A Natural F Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Tensile Strength at Break | 77.9 MPa | 11300 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ 600 A Natural Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Tensile Strength at Break | 77.9 MPa | 11300 psi | ASTM D638 |
LNP Thermocomp® FP-VC-1003 BK8-019 Polyvinylidene Fluoride, Carbon Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Tensile Strength at Break | 77.9 MPa | 11300 psi | |
Abatron AboCast 8103-22 High-Performance Dielectric Epoxy AboCast 8103-22 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system is used in.. |