Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 69.98 MPa | 10150 psi | ISO 527-1 |
MRC Polymers NAXALOYâ„¢ 770 GF10 ABS+PC Alloy, 10% Glass Fiber Filled Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Tensile Strength at Break | 69.98 MPa | 10150 psi | ASTM D638 |
Aclo Accucomp Polycarbonate POL051L Medium Viscosity |
|||
Tensile Strength at Break | 69.98 MPa | 10150 psi | ASTM D638 |
Aclo Accuguard Polycarbonate POL050G10HIV0L Glass Reinforced High Impact Flame Retardant |
|||
Tensile Strength at Break | 69.98 MPa | 10150 psi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0339G30CL Glass Reinforced Coupled |
|||
Tensile Strength at Break | 69.98 MPa | 10150 psi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0336G30CL Glass Reinforced Coupled |