Polymer Property : Tensile Strength at Break = 655 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 655 MPa
95000 psi
Annealed
Hoskins Manufacturing Chromel® Thermocouple Wire
Used in Type E and Type K thermocouples. All values may vary dependent on specific design and usageChromel® is a registered trade name of Hoskins Manufacturing.Capabilities: WireRibbonSquareInsu..
Tensile Strength at Break 655 MPa
95000 psi
Stress relieved
Special Metals MONEL® 404 Copper-Nickel Alloy
Data provided by California Fine Wire and the manufacturer, Special Metals.
Tensile Strength at Break 655 - 827 MPa
95000 - 120000 psi
ThyssenKrupp X8Ni9 Structural Steel
Data applies to plate thicknesses from 13/64 to 1 15/64 in.9% nickel steel for low temperature service down to -320°FApplication for pressure vessels and tanks for the transportation and storage of..
Tensile Strength at Break 655 MPa
95000 psi
Annealed
California Fine Wire Stablohm 675 Nickel, Chromium and Iron Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break >= 655 MPa
>= 95000 psi
Carlson Nitronic® 60® Austenitic Stainless Steel
General DescriptionNitronic 60 is an anti-galling and wear resistant austenitic stainless steel. It provides a significantly lower cost alternative to combat wear and galling when compared with cob..
Tensile Strength at Break >= 655 MPa
>= 95000 psi
Carlson Nitronic® 30® Austenitic Stainless Steel
General DescriptionNitronic 30 is a nitrogen-strengthened austenitic stainless steel developed for applications requiring good aqueous corrosion resistance combined with good resistance to abrasive ..