Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 65.5 MPa | 9500 psi | 2 in/min; ASTM D638 |
RheTech Products GC30P200-01UV 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, Black Applications: Interior componentsStructural housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 65.5 MPa | 9500 psi | chs 2 in/min; ASTM D638 |
Network Polymers MS 100 Styrene Methyl Methacrylate Copolymer Description: Styrene Methyl Methacrylate CopolymerInformation provided by Network Polymers Inc. |
|||
Tensile Strength at Break | 65.5 MPa | 9500 psi | ASTM D638 |
Polymer Resources PC-G10 Polycarbonate, 10% Glass Reinforced Polycarbonate, 10% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Tensile Strength at Break | 65.5 MPa | 9500 psi | ASTM D638 |
Polymer Resources PC-G10-[color]-1 Polycarbonate, 10% Glass Reinforced with Mold Release Polycarbonate, 10% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Tensile Strength at Break | 65.5 MPa | 9500 psi | TM R050-36 |
Resinlab® EP950G Gray Aluminum Filled Rubber Modified Epoxy EP950G Gray is an aluminum filled one part rubber modified epoxy designed for bonding metal and other structural material subject to stress at elevated temperature. It is a medium paste-like viscosi.. |
|||
Tensile Strength at Break | 65.5 MPa | 9500 psi | ASTM D638 |
Polymer Resources PC-FD4 Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Tensile Strength at Break | 65.5 MPa | 9500 psi | ASTM D638 |
Polymer Resources PC-HM-FR1-[color]-TFE Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear Resistant Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes.. |
|||
Tensile Strength at Break | 65.5 MPa | 9500 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N1000EL Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago. |
|||
Tensile Strength at Break | 65.5 MPa | 9500 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 2061-22 Polycarbonate Resin Overview: CALIBREâ„¢ 2061-22 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-22 provides exceptional clarity, heat resistance, impa.. |
|||
Tensile Strength at Break | 65.5 MPa | 9500 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 302EP-22 Polycarbonate Resin Overview: CALIBREâ„¢ 300EP-22 Series are polycarbonate resins that offer exceptional impact resistance, heat distortion resistance and optical clarity for injection molding applications. Their hi.. |
|||
Tensile Strength at Break | >= 65.5 MPa | >= 9500 psi | |
Master Bond EP30P Epoxy Bonds Glass, Polycarbonates and Acrylics Description: Master Bond Polymer Adhesive EP30P is a two component, transparent, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulating and casting. It is for.. |
|||
Tensile Strength at Break | >= 65.5 MPa | >= 9500 psi | |
Master Bond Supreme 10HTCL Epoxy for Cryogenic Applications Description: Master Bond Supreme 10HTCL features a blend of performance properties including both high shear and peel strengths along with convenient handling. This one component system is formulate.. |
|||
Tensile Strength at Break | 65.5 MPa | 9500 psi | ASTM D638 |
Plastics Group Polifil® GFABS-10 10% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS) Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire.. |
|||
Tensile Strength at Break | 65.5 MPa | 9500 psi | ASTM D638 |
Chase Plastics CP Pryme® NN100L (COND, 50% RH) Nylon 66, Internally Lubricated Information provided by Chase Plastics. |
|||
Tensile Strength at Break | >= 65.5 MPa | >= 9500 psi | |
Master Bond EP30LV Optically Clear, Low Viscosity Epoxy Adhesive Description: Master Bond Polymer System EP30LV is a low viscosity, two component epoxy adhesive for general purpose bonding, coating, sealing and casting formulated to cure at room temperature or mo.. |
|||
Tensile Strength at Break | >= 65.5 MPa | >= 9500 psi | |
Master Bond EP30LV-1 Ultra Low Viscosity, Two Part Epoxy System Description: Master Bond Polymer System EP30LV-1 is an ultra low viscosity, two component epoxy system for high performance bonding, coating, sealing, potting and encapsulation. It readily cures at .. |
|||
Tensile Strength at Break | 65.5 MPa | 9500 psi | ASTM D638 |
Entec Hylex® P1310FR Polycarbonate Information provided by Ravago |
|||
Tensile Strength at Break | 65.5 MPa | 9500 psi | ASTM D638 |
Entec Hylex® P1025L2 HB Polycarbonate Available in North America Additive: Mold Release Features: Good Mold Release and High Flow RoHS Compliant Form: Pellets Appearance: Blue Information provided by Entec |
|||
Tensile Strength at Break | 65.5 MPa | 9500 psi | ASTM D638 |
Polymer Resources PPX-GP7 Modified PPO, General Purpose with HDT of 300 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |