Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 320 MPa | 46400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP LC00APXQ PEEK LNP* THERMOCOMP* LC00APXQ is a compound based on Polyetheretherketone resin containing 50% Carbon Fiber. Added features of this material include: Exceptional Processing, Electrically Conductive. |
|||
Tensile Strength at Break | 320 - 740 MPa | 46400 - 107000 psi | |
Goodfellow Phosphor Bronze Good Machinability. Uses include springs, clips, gauzes and architectural applicationsInformation provided by Goodfellow. |
|||
Tensile Strength at Break | 320 - 620 MPa | 46400 - 89900 psi | |
Goodfellow Platinum 90/Rhodium 10 Thermocouple Alloy The positive element of the type S thermocouple. Type S thermocouples are characterized by a high degree of chemical inertness and stability at high temperatures. Often used as a standard for calibr.. |