Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 3.50 MPa | 508 psi | ISO 37 |
PolyOne OnFlex™ S KG 60A-3S2018 Thermoplastic Elastomer (TPE) OnFlex™-S KG thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Tensile Strength at Break | <= 3.50 MPa | <= 508 psi | ISO/R527 |
Polykemi AB POLYelast TPE Z300 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Tensile Strength at Break | 3.50 MPa | 508 psi | |
Shin-Etsu Silicones KE-1204 A Silicone, Potting/Encapsulation RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tensile Strength at Break | 3.50 MPa | 508 psi | After Curing |
Silikony Polskie Polastosil M-33 Silicone Rubber Medium hard with good tearing resistance |
|||
Tensile Strength at Break | 3.50 MPa | 508 psi | ASTM D412 |
Sumitomo Chemical ESPOLEX® WT446 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Tensile Strength at Break | 3.50 MPa | 508 psi | ISO 37 |
ELASTO UK Dryflex® 8014-101 Flame Retardant TPE for Extrusion, Black Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and.. |
|||
Tensile Strength at Break | 3.50 MPa | 508 psi | ISO 37 |
ELASTO UK Dryflex® 8014-101 Flame Retardant TPE for Injection Molding, Black Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu.. |
|||
Tensile Strength at Break | 3.50 MPa | 508 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 211-45 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Tensile Strength at Break | 3.50 MPa | 508 psi | ISO 527-1 |
Barlog Plastics KEBAFLEX E 40.1 TPE-V, Shore A40 TPE-VInformation provided by BARLOG plastics GmbH. |
|||
Tensile Strength at Break | <= 3.50 MPa | <= 508 psi | ISO/R527 |
Polykemi AB POLYelast TPE Z557 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Tensile Strength at Break | 3.50 MPa | 508 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 111-45 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |